MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Norplex-Micarta RT630H Phenolic Paper Laminate Tube, NEMA XXX
Categories: Polymer; Thermoset; Phenolic

Material Notes: Being a heat treated version of RT630, RT630H is a fine machining grade with excellent electrical properties and moisture resistance. It has good dimensional stability and resists splitting. Typical applications include fuse tubes, coil forms and supports.

Information provided by Norplex-Micarta

Key Words: Paper, Phenolic, Micarta, NEMA XXX, MIL-I-24768/10 Type PBE, ASTM D709 Type I Grade XXX
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/cc0.750" X 1.000"; ASTM D792
Moisture Absorption 0.700 %0.700 %0.750" X 1.000"; ASTM D570 Condition D1-24/23
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 1101100.750" X 1.000"; ASTM D785
Tensile Strength 107 MPa15500 psi0.750" X 1.000"; ASTM D638 Condition A
Compressive Strength 165 MPa24000 psi0.750" X 1.000"; ASTM D695 Condition A
Compressive Modulus 2.59 GPa375 ksi0.750" X 1.000"; ASTM D695 Condition A
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 13.8 kV/mm350 kV/in0.750" X 1.000"; ASTM D149 Condition D-48/50
 19.7 kV/mm500 kV/in0.750" X 1.000"; ASTM D149 Condition A
Dielectric Breakdown 29000 V29000 V0.750" X 1.000"; ASTM D149 Condition D-48/50
 80000 V80000 V0.750" X 1.000"; ASTM D149 Condition A
 
Thermal PropertiesMetricEnglishComments
UL RTI, Electrical 140 °C284 °F0.750" X 1.000"; UL Bulletin 746b
UL RTI, Mechanical with Impact 130 °C266 °F0.750" X 1.000"; UL Bulletin 746b
Flammability, UL94 HBHB0.750" X 1.000"

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Norplex-Micarta NP610 Phenolic Paper Laminate Sheet, NEMA X
Norplex-Micarta RT630S Phenolic Paper Laminate Tube, NEMA XXX
Norplex-Micarta NP629 Phenolic Paper Laminate Sheet, NEMA XX
Norplex-Micarta RT630 Phenolic Paper Laminate Tube, NEMA XXX
Norplex-Micarta RT628H Phenolic Paper Laminate Tube, NEMA XX

PNORPM105 / 192844

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.