MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Monprene® OM-12265-01 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene OM-12265-01 is a specialty thermoplastic elastomer designed for overmolding applications like grips and anti-skid parts for consumer and industrial products. Monprene OM-12265-01 is a medium hardness, low density, UV stabilized grade that exhibits excellent adhesion to PC, ABS and PC/ABS.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Bondability; Good Adhesion; Good Moldability; Light Stabilized; Lubricated; Medium Flow; Low Density; Low Specific Gravity; Medium Hardness; Slip; UV Resistant

Uses: Appliances; Bonding; Cell Phones; Flexible Grips; Handles; Knobs; Overmolding; Power/Other Tools; Rubber Replacement; Sporting Goods; Writing Instruments

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Multi Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ASTM D792
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  66
@Time 5.00 sec
66
@Time 0.00139 hour
Injection Molded; ASTM D2240
 68
@Time 1.00 sec
68
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 6.21 MPa900 psiASTM D412
Elongation at Break 600 %600 %ASTM D412
 
Processing PropertiesMetricEnglishComments
Processing Temperature 188 - 216 °C370 - 420 °FMelt, Injection
Rear Barrel Temperature 188 - 216 °C370 - 420 °F
Middle Barrel Temperature 188 - 216 °C370 - 420 °F
Front Barrel Temperature 188 - 216 °C370 - 420 °F
Nozzle Temperature 188 - 216 °C370 - 420 °F
Mold Temperature 15.6 - 32.2 °C60.0 - 90.0 °F
Drying Temperature 60.0 °C140 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Injection Pressure 1.38 - 5.52 MPa200 - 800 psi
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceNatural Color
 Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0908 / 237399

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.