MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials Pearlcoat® Activa D198K Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP

Material Notes: PEARLCOAT® Activa D198K is an aliphatic based thermoplastic polyurethane of low hardness, supplied in form of natural pellets. This product gives an inherent “low gloss aspect” on the final product surface after extrusion processing. Featuring low gel content as well as low temperature flexibility, it is ideally suited for extrusion or co-extrusion onto polar substrates.

All information provided by Merquinsa

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70ASTM D2240
Tensile Strength, Yield 3633 psiASTM D412
Elongation at Break 455 %ASTM D412
50% Modulus 4.00 MPa
@Strain 50 %
ISO 527-2/5A/500
100% Modulus 0.843 ksi
@Strain 100 %
ASTM D412
300% Modulus 1.889 ksi
@Strain 300 %
ASTM D412
Tear Strength 314 pliUnnicked; ASTM D624 (die C)
Abrasion 30Resistance [mm^3]; ISO 4649-A
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 46.0 °CISO 306 (A50)
 
Processing PropertiesOriginal ValueComments
Zone 1 185 - 205 °C
Zone 2 190 - 210 °C
Zone 3 195 - 215 °C
Zone 4 190 - 210 °C
Adapter Temperature 185 - 210 °C5
Die Temperature 185 - 205 °C(6)
 185 - 205 °CTIP (7)
Drying Temperature 90.0 °C
Dry Time 3.00 hour
Dew Point <= -30.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Elastamax™ XL-2055 Thermoplastic Polyolefin Elastomer (TPO (POE))
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer
Barlog Plastics KEBAFLEX S 45 A.01 TPE-S, Shore A45, translucent
Lubrizol Advanced Materials Pearlthane® D91F88 Thermoplastic Polyurethane Elastomer
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer

PMES78 / 101322

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.