MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Master Bond UV15X-6NM-2 One Component UV Curing Urethane Acrylate
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Key Features:
  • Outstanding abrasion resistance
  • Superior non-yellowing properties
  • Excellent flexibility and toughness
  • Moderate viscosity
Product Description: Master Bond UV15X-6NM-2 is a one component, UV curing urethane acrylate system featuring vibrant flexibility, excellent toughness and superior abrasion resistance. This moderate viscosity compound can be used for a wide variety of applications including bonding, sealing, coating and encapsulation. Its robust flexibility gives it the capacity to withstand severe thermal cycling as well as resisting thermal and mechanical shocks. UV15X-6NM-2 bonds well to a variety of substrates including glass, plastics including polycarbonates and acrylics, composites, metals and many types of rubbers. It has very good chemical resistance, especially to water, cleaning agents and oils. UV15X-6NM-2 is a top notch thermal and electrical insulator with a service temperature range of -80°F to +250°F. It should be noted that it has a substantial non-yellowing profile. UV15X-6NM-2 generally cures readily in 10-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm². The rate of cure depends upon the system’s distance from the light source, the thickness of the section and the intensity of the light source. It should be noted that the system can cure in sections approaching 1/4 inch thick. However, when bonding, sections of a few thousandths of an inch are more than adequate. Most importantly, UV15X-6NM-2 does not display oxygen inhibition. This system is widely used in fiber-optic, optical, electronic, semiconductor, microelectronic and laser applications..

Product Advantages:

  • One part system with no mixing needed
  • Cures very fast upon exposure to 320-365 nm UV light at ambient temperatures
  • No oxygen inhibition
  • Highly reliable thermal and electrical insulator
  • Outstanding flexibility, toughness and abrasion resistance
  • Performs well in withstanding rigorous thermal cycling as well as thermal and mechanical shocks
  • Superb non-yellowing capabilities

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/cc
Viscosity 35000 - 55000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 25 - 35
Tensile Strength 1800 - 2000 psi
Elongation at Break >= 200 %
Tensile Modulus 100000 - 150000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+12 ohm-cm
Dielectric Constant 4.5
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -80.0 °F
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.50
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature <=23.9 °C
in original, unopened containers
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Fusabond® EB560D Ethylene Acrylate Terpolymer
Avient Edgetek® ET3500-5002 BK Acrylonitrile Styrene Acrylate + PC (ASA+PC)
Avient Edgetek® ET3500-5001 colored Acrylonitrile Styrene Acrylate + PC (ASA+PC)
Borosilicate Glass
Master Bond UV15-7 One Part UV Curable Polymer

PMASTM977 / 185570

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.