Notes: Monprene IN-12490 is a general purpose thermoplastic elastomer, available in NAT and BLK, designed for a variety of industrial applications, including seals and gaskets. Monprene IN-12490 is high hardness, low density, UV stable grade suitable for injection molding and extrusion. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Light Stabilized; Low Flow; High Hardness; Low Density; Low Specific Gravity; Lubricated; Slip; Sunlight Resistant; Without Filler Uses: Consumer Applications; Gaskets; Handles; Industrial Applications; Sporting Goods; Tubing; Writing Instruments RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding; Extrusion Information provided by Teknor Apex |