Wave Solder Flux 3590-TX is a low-solids, non-halide rosin/resin free flux designed to eliminate post-cleaning operations. Very effective flux activators provide superior solderability, reduced defects and shiny solder joint formation. 3590-TX has a wide process window with excellent wetting capabilities, leaving no residue and high surface insulation resistance.Features - Eliminates the need for cleaning
- Good solderability
- Low defects
- Compatible with conformal coatings without cleaning
- Meets Bellcore Specification TR-NWT-000078
Physical Properties - Color: Clear
- Flux Type Classification: ORL0
Information Provided by Indium Corporation |