MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik 23.7.L Welding wire
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik 23.7.L is a duplex stainless filler metal for welding lean duplex stainless steels such as Sandvik SAF 2304, LDX 2101* and similar. Corrosion resistance is equal to 316L in most applications.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 230TIG
Tensile Strength, Ultimate 600 MPaSAW, FLUX 15W
 710 MPaTIG
Tensile Strength, Yield 500 MPa
@Strain 0.2 %
SAW, FLUX 15W
 525 MPa
@Strain 0.2 %
TIG
Elongation at Break 25 %TIG
 30 %SAW, FLUX 15W
Charpy Impact 90.0 J
@Temperature -20.0 °C
SAW, FLUX 15W
 100 J
@Temperature 20.0 °C
SAW, FLUX 15W
 150 J
@Temperature -20.0 °C
TIG
 170 J
@Temperature 20.0 °C
TIG
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.5 µm/m-°C
@Temperature 20.0 - 400 °C
Thermal Conductivity 16.0 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.020 %
Chromium, Cr 23 %
Manganese, Mn 1.7 %
Molybdenum, Mo 0.30 %
Nickel, Ni 7.0 %
Nitrogen, N 0.14 %
Phosphorus, P <= 0.025 %
Silicon, Si 0.70 %
Sulfur, S <= 0.0050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSANDV5120 / 199684

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.