MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ixom ALKATEQ™ SHE2000 LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: ALKATEQ™ SHE2000 is a linear low-density polyethylene (LLDPE) sheathing compound specifically designed for use in manufacture of both above and below ground cables. SHE2000 provides optimal processing performance for sheathing of cables and also provides an excellent surface finish to the extruded cable. SHE2000 is compounded with antioxidants and a high-quality, well-dispersed carbon black pigment to provide excellent outdoor weathering performance. ALKATEQ™ SHE2000 complies with the requirements of AS1049 for polyethylene sheath or jacket material.

Information provided by Ixom Operations PTY LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³base polymer; ASTM D1505
ESCR 10% Igepal® >= 5000 hour
@Temperature 50.0 °C
>= 5000 hour
@Temperature 122 °F
IEC 60811-4-1/B
Oxidative Induction Time (OIT) >= 75 min
@Temperature 200 °C
>= 75 min
@Temperature 392 °F
ASTM D638
Absorption Coefficient 440440[ab/mm] 375 nm; ASTM D3349
Carbon Black Loading 2.6 %2.6 %AS 1049.2
Melt Flow 0.85 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.85 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 18.0 MPa>= 2610 psiType IV specimen @ 50mm/min; ASTM D638
Elongation at Break >= 60 %>= 60 %Type IV specimen @ 50mm/min; ASTM D638
 
Descriptive Properties
Carbon Black Dispersion2Grading, ISO 18553
 A2Appearance, ISO 18553

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PIXOM011 / 283092

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.