MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Multibase Multi-Pro® 4003 R Medium Impact 40% Glass Filled Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Glass Fiber Filler

Material Notes: Moisture content is 0.06%. Multi-Pro 4003 R is a glass reinforced polypropylene compound featuring extremely high stiffness and high impact resistance. Suitable for engineering applications and automotive heat resistant parts under the hood.

Data provided by Multibase.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccASTM D792-91
Melt Flow 3.0 g/10 min(Condition L) ASTM D-1238-94a
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 7710 sec; ASTM D-2240-95
Tensile Strength, Ultimate 54.5 MPaASTM D638-95
Elongation at Break 2.0 %ASTM D638-95
Flexural Strength 69.0 MPaASTM D790-95
Flexural Modulus 5.517 GPaMethod 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 0.640 J/cmASTM D256-93a
Gardner Impact 0.300 JASTM D5420-93
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 147 °CASTM D648-95
Deflection Temperature at 1.8 MPa (264 psi) 140 °CASTM D648-95

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Entec Hypro™ F PPH-GF40 Natural Homopolymer Polypropylene, 40% Glass Reinforced
Ravago Manufacturing Americas Echo® RPC40G BK Polypropylene Homopolymer
Multibase Multi-Pro® 4008 RC Medium Impact 40% Glass Filled Polypropylene
RheTech Products G40P100-01 40% Glass Fiber Reinforced Polypropylene, Black
A. Schulman Gapex® RPP30DA10BK 30% Fiberglass Reinforced, Heat Stabilized, Homopolymer Polypropylene

PLA282 / 49679

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.