HMW-Bimodal Resin Applications: T-shirt bags, trash can liners, heavy duty bags Formolene E905 is a high molecular weight grade of HDPE with well-balanced strength in both the machine (MD) and transverse (TD) directions and good stiffness characteristics. Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact. Information provided by Formosa Plastics Corporation, USA. |