MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Manifattura Cattaneo POM c Acetal
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.

Information provided by Manifattura Cattaneo s.p.a.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccISO 1183
Moisture Absorption at Equilibrium 0.20 %
@Temperature 23.0 °C
50% RH; ISO 62
Water Absorption at Saturation 0.85 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 84ISO 2039-2
Tensile Strength, Yield 63.0 MPaISO 527
Elongation at Break 33 %ISO 527
Elongation at Yield 10 %ISO 527
Tensile Modulus 2800 MPaISO 527
Flexural Strength 89.0 MPa
Flexural Modulus 2500 MPaISO 178
Compressive Yield Strength 19.0 MPa
@Strain 1 %
ISO 604
Poissons Ratio 0.43
Charpy Impact Unnotched 280 kJ/m²ISO 179
Charpy Impact, Notched 8.00 kJ/m²ISO 179
Coefficient of Friction, Dynamic 0.21on polished steel; MPC Test
Coefficient of Friction, Static 0.14on polished steel; MPC Test
K Factor (Wear Factor) 3.8µm/s. PV = 0.1 MPa-m/s; max P = 18 MPa; MPC Test
Limiting Pressure Velocity 0.150 MPa-m/secwithout lubrication; MPC Test
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohmIEC 60094
Dielectric Constant 3.9
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 22.0 kV/mm
@Thickness 2.00 mm
IEC 60243
Dielectric Loss Index 0.0070
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 110 µm/m-°C
@Temperature 23.0 - 100 °C
ASTM D696
Thermal Conductivity 0.310 W/m-KDOM 52612
Maximum Service Temperature, Air 115 °C
Deflection Temperature at 0.46 MPa (66 psi) 156 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 105 °CISO 75
Flammability, UL94 HB
 V-2
Oxygen Index 15 %ISO 4589
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
ColorBlack
 White
UV ResistanceN

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUCEL N109-02 General Purpose POM, Unreinforced, Externally Lubricated, Standard Viscosity
Avient LubriOne™ AT-000/05T Acetal (POM) Copolymer
DuPont Mobility and Materials Delrin® 100 NC010 POM
KEP Kepital® F20 Acetal Copolymer
Kolon KOCETAL® K200 Standard Grade Acetal Resin

PMANIF905 / 156185

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.