MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman Fiberfil® J-60/20/E8/M Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Information provided by FIBERFIL Engineered Plastics, now an A. Schulman product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccASTM D792
Water Absorption 0.030 %24 hr; ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
@Thickness 3.17 mm
ASTM D955
 0.0040 cm/cm
@Thickness 6.35 mm
ASTM D955
Melt Flow 9.0 g/10 min230/2.16 (typical); ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100 - 110ASTM D785
Tensile Strength, Yield 10000 psiASTM D638
Elongation at Yield 3.5 %ASTM D638
Tensile Modulus 600000 psiASTM D638
Flexural Strength 13500 psiASTM D790
Flexural Modulus 550 ksiTangent; ASTM D790
Izod Impact, Notched 1.20 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 315 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 300 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 390 - 410 °F
Middle Barrel Temperature 400 - 440 °F
Front Barrel Temperature 360 - 390 °F
Nozzle Temperature 360 - 380 °F
Melt Temperature 390 - 450 °F
Mold Temperature 90.0 - 160 °F
Drying Temperature 170 °FDrying not normally required
Dry Time 2 hourDrying not normally required
Moisture Content <= 0.20 %recommended for molding
Back Pressure 0.000 - 100 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 128 HI Z  Polypropylene (PP) Talc 20% - High Impact - FDA Type
A. Schulman Fiberfil® J-60/20/TT/FD WT8381 Polypropylene Homopolymer, 20% Glass Reinforced, FDA compliant
LG Chemical LUPOL GP2200 PP+GF20%
A. Schulman Gapex® FPP20GQ12HB 20% Fiberglass/Mineral Reinforced, Chemically-Coupled, Impact-Modified Polypropylene
A. Schulman Fiberfil® J-69/20/E High performance polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled

PFIBFIL60 / 38245

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.