MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Schott ZERODUR® Glass Ceramic
Categories: Ceramic; Glass; Optical

Material Notes: ZERODUR® is a glass ceramic with an extremely low thermal expansion for demanding applications in which geometrical shape and distance changes must kept smallest possible under temperature variations. The key properties of ZERODUR® are:
  • Extremely low coefficient of thermal expansion (CTE) for a wide temperature range
  • Excellent CTE homogeneity throughout the total volume
  • Very low content of imperfections
  • Wide range of precise geometrical Shapes
  • Extremely smooth surface with residual roughness below 1 nm
Uses:
  • Stages and mirrors for lithography equipment
  • Mirror substrates for segmented and monolithic large astronomical telescopes
  • Ultra light weighted mirror blanks
  • High precision mechanical parts, e.g. ring laser gyroscope bodies
  • Reference standards for precision measurement technology and comet probes

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.53 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 6200.1/20
Modulus of Elasticity 90.3 GPa
Poissons Ratio 0.24
Shear Modulus 36.4 GPaCalculated
 
Thermal PropertiesOriginal ValueComments
CTE, linear 0.000 - 0.00700 µm/m-°C
@Temperature 0.000 - 50.0 °C
EXTREME
 0.000 - 0.0100 µm/m-°C
@Temperature 0.000 - 50.0 °C
SPECIAL
 0.000 - 0.0200 µm/m-°C
@Temperature 0.000 - 50.0 °C
class 0
 0.0100 - 0.0300 µm/m-°C
@Temperature 0.000 - 50.0 °C
Homogeneity
 0.000 - 0.0500 µm/m-°C
@Temperature 0.000 - 50.0 °C
class 1
 0.000 - 0.100 µm/m-°C
@Temperature 0.000 - 50.0 °C
class 2
Specific Heat Capacity 0.800 J/g-°C
Thermal Conductivity 1.45 W/m-K
Maximum Service Temperature, Air 600 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schott ZERODUR® K20 Glass Ceramic
Mateck Zero Expansion Glass - ZERODUR
CeramTec Sikor® S Cordierite
Carpenter Invar 36® Alloy, Cold Drawn Bars
DuPont Mobility and Materials Delrin® 150 NC010 POM

CSGT9948 / 183201

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.