MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ATI Allegheny Ludlum AL 17-4 High Strength Stainless Steel, UNS S17400
Categories: Metal; Ferrous Metal; Stainless Steel; Precipitation Hardening Stainless

Material Notes: ATI 17-4™ precipitation hardening stainless steel (S17400), Type 630, is a chromium-nickel-copper precipitation hardening stainless steel used for applications requiring high strength and a moderate level of corrosion resistance. High strength is maintained to approximately 600°F (316°C). This alloy is designated Grade or Type 630 in several specifications. The S17400 alloy is martensitic in structure in the annealed condition and is further strengthened by a low temperature treatment which precipitates a copper containing phase in the alloy. In comparison to many alloys in the precipitation hardening family, the S17400 alloy requires a simple heat treatment; a one step process conducted at a temperature in the range 900°F (482°C) to 1150°F (621°C) depending on the combination of strength and toughness desired. A wide range of properties can be produced by this one step heat treatment. Heat treatment in the 900°F (482°C) range produces highest strength, although slightly less than that of alloys like S17700 or S15700. The latter precipitation hardening stainless steels generally require more steps to complete heat treatment.

Key Words: DIN 1.4548; ASTM A-693; ASME SA-693; AMS 5604, 17-4PH, 17/4PH, 17-4 PH; formerly sold under the Allvac® Vasco® 17-4 trade names
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.76 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 33
Tensile Strength, Ultimate 1030 MPa
Tensile Strength, Yield 760 MPa
@Strain 0.2 %
Elongation at Break 8.0 %
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr 17 %
Copper, Cu 3.5 %
Iron, Fe 75.5 %as balance
Nickel, Ni 4.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
316 Stainless Steel, annealed bar
Industeel VIRGO 17.4PH 17Cr-4Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (496°C - 4 hours + air cooled)
Titanium Ti-6Al-4V (Grade 5), Annealed
FloMet 17-4PH Stainless Steel, Heat Treated (H-900)
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition A

NLP174 / 18033

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.