MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales
metalmen Is Your Direct to US Manufacturing Source for High Purity Metals

(Viewing data as-entered. Click here to return)
Tetracalcium-Phosphate, Ca4PO9
Categories: Ceramic; Oxide; Wood and Natural Products

Material Notes: Tetracalcium-Phosphate is a natural constituent of teeth and bone, along with other calcium-phosphate ceramic (CPC) materials such as hydroxyapatite. Synthetic calcium-phosphate ceramics are used as an active bioceramic for teeth and bone replacement.

Key Words: Ca4PO9
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.10 g/cc
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 120 - 200 MPa

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Calcium Hydroxyapatite, Ca10(PO4)6(OH)2
Tricalcium-Phosphate (TCP), CA3(PO4)2
Diamond, Natural
American Black Ash (Brown Ash) Wood
American Pine Wood

BBIOC01 / 150

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.