MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Rogers Arlon 680-R3844R 0.084" (2.13 mm) Cured Silicone Coating with Silica-based Substrate
Categories: Polymer; Thermoset; Silicone

Material Notes: Design/Construction:
Side 1: Cured Silicone Coating
Substrate: Silica-based
Side 2: Cured Silicone Coating Rubber
    Application Advantages:
  • Extremely low thermal conductivity
  • Thermally stable
  • Bondable to silicone rubber
  • 2-3 times thinner than competing silicone foam
  • Flexible and light weight
  • Energy savings
Recommended process method for particle free applications: Vacuum Bag Cure Cycle: 15 minutes @ 250°F under 15 psi-Oversized uncured silicone rubber to seal the exposed edges

Product Use: Thermal insulation

Appearance: Red silicone rubber on black fabric

This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 2.00 milSide 1; Arlon SQA-TMS-003
 2.00 milSide 2; Arlon SQA-TMS-003
 80.0 milSubstrate; Arlon SQA-TMS-003
 84.0 milOverall; Arlon SQA-TMS-003
 
Mechanical PropertiesOriginal ValueComments
Peel Strength >= 1.00 plito Arlon 51270R015, Bond Strength; Arlon SQA -TMS-011
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0300 W/m-K
@Temperature 200 °C
Arlon SQA-TMS-022
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air 18.3 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 min
@Pressure 0.103 MPa,
Temperature 121 °C
Recommended Cure Cycle
Shelf Life 60.0 Month
@Temperature 21.1 °C
From date of manufacture
 
Descriptive Properties
ColorDark Red
Total Product Weight (oz/yd2)15.7Arlon SQA-TMS-025
Uncoated Fabric Break Strength18 lb/inWrap Direction, Arlon SQA-TMS-026

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PARL432 / 125618

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.