MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Conventus Polymers Duramide™ PA66GF33HI Nylon 66, 33% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Duramide PA66GF33HI is a glass fiber reinforced PA66 with impact modification developed for applications that require high strength and improved low temperature impact over standard glass filled PA66. It also contains a lubricant package for easy molding. Available in colors.

Information provided by Conventus Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/ccASTM D792
Water Absorption 0.50 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.00035 in/in
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 22500 psiASTM D638
Elongation at Break 4.0 %ASTM D638
Flexural Strength 30000 psiASTM D790
Flexural Modulus 1.00e+6 psiASTM D790
Izod Impact, Notched 1.90 ft-lb/in
@Thickness 3.17 mm,
Temperature -40.0 °C
ASTM D256
 3.20 ft-lb/in
@Thickness 3.17 mm,
Temperature 22.8 °C
ASTM D256
Izod Impact, Unnotched 26.0 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µin/in-°FASTM D696
Maximum Service Temperature, Air 530 °F
 550 °F
Deflection Temperature at 1.8 MPa (264 psi) 415 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 540 °F
Mold Temperature 175 - 220 °F
Drying Temperature 180 °F
Dry Time 2.00 - 4.00 hour
Moisture Content <= 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Capron® 5233G 33% Glass-Filled Nylon 66 (Dry)
Celanese Zytel® 70G33L BK031 PA66-GF33
Nylene® 9633 33% Glass Reinforced Nylon 6,6/6
Nylene® Nylene 5133 HS Nylon 66, Glass Reinforced, Impact Grade
BASF Ultramid® 1503-2 BK ND3007 33% Glass Filled PA66 (Conditioned)

PCONV917 / 233817

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.