System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
DuPont Mobility and Materials Zytel® 8018HS NC010 PA66-IGF14
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, 10% Glass Fiber Filled
Material Notes:
14% Glass Reinforced, Toughened, Heat Stabilized, Polyamide 66
While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.19
g/cc
DAM; ISO 1183
Water Absorption
6.3 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption
1.90 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow
0.0040
cm/cm
DAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse
0.0080
cm/cm
DAM; ISO 294-4, 2577
Mechanical Properties
Original Value
Comments
Hardness, Rockwell M
70
DAM; ISO 2039-2
Hardness, Rockwell R
110
DAM; ISO 2039-2
Tensile Strength at Break
58.0
MPa
50% RH; ISO 527-1/-2
85.0
MPa
DAM; ISO 527-1/-2
Elongation at Break
6.0 %
DAM; ISO 527-1/-2
14 %
50% RH; ISO 527-1/-2
Tensile Modulus
2300
MPa
50% RH; ISO 527-1/-2
4200
MPa
DAM; ISO 527-1/-2
Flexural Modulus
2000
MPa
50% RH; ISO 178
3600
MPa
DAM; ISO 178
Poissons Ratio
0.36
DAM; ISO 527-1/-2
0.39
50%RH; ISO 527-1/-2
Izod Impact, Notched (ISO)
70.0
kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1U
90.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1U
90.0
kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1U
100
kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1U
Izod Impact, Unnotched (ISO)
5.00
kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
5.00
kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
7.00
kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
10.0
kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
13.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
18.0
kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched
75.0
kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
80.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
80.0
kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
100
kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched
4.00
kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
4.00
kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
6.00
kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
6.00
kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
14.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
18.0
kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
Electrical Properties
Original Value
Comments
Comparative Tracking Index
580
V
DAM; IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
50.0
µm/m-°C
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow
118
µm/m-°C
DAM; ISO 11359-1/-2
Melting Point
263
°C
10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi)
246
°C
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi)
195
°C
DAM; ISO 75-1/-2
Flammability, UL94
HB
@Thickness 0.750 mm
DAM; IEC 60695-11-10
HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
Flame Spread
<=
80.0
mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
Oxygen Index
21 %
DAM; ISO 4589-1/-2
Processing Properties
Original Value
Comments
Melt Temperature
285
-
305
°C
Injection
295
°C
Injection Optimum
Mold Temperature
50.0
-
100
°C
Injection
80.0
°C
Injection Optimum
Ejection Temperature
210
°C
Injection
Drying Temperature
80.0
°C
Injection
Dry Time
2.00
-
4.00
hour
Dehumidified Dryer; Injection
Moisture Content
0.20 %
Injection
Hold Pressure
50.0
-
100
MPa
Injection
Descriptive Properties
Additives
Release agent
Delivery form
Pellets
Drying Recommended
yes
Injection
FMVSS Class
B
ISO 3795 (FMVSS 302)
Hold pressure time (s/mm)
3
Injection
Max. screw tangential speed (m/s)
0.2
Injection
Part Marking Code
PA66-IGF14
ISO 11469
Processing
Injection Molding
Regional Availability
North America
South and Central America
Resin Identification
PA66-IGF14
ISO 1043
Special characteristics
Heat stabilized or stable to heat
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Ascend Performance Materials Vydyne® R413H NT Impact Modified Nylon 66, Glass Filled
Ravago Manufacturing Americas Hylon® N1013HL Nylon 6/6 (Cond)
Celanese Zytel® 8018HS BKB085 PA66-IGF14
EMS-Grivory Grilon® BGZ-30/2 PA6-GF30
Ravago Manufacturing Americas Hylon® N1013THL Nylon 6/6 (DAM)
PDSX5375 / 198015
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.