Description: Extra high izod impact, very high flexural modulus, good low temperature drop impact. Applications: Suggested uses include compounding and thermoforming. Process: Thermoforming. This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDA. Information provided by Braskem |