MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CMT Materials HYTAC® B1X High Durability Thermoplastic Syntactic
Categories: Polymer

Material Notes: HYTAC-B1X is the first plug assist material to combine the toughness of an engineered thermoplastic with the low thermal conductivity of syntactic foam. Plug assist made from HYTAC-B1X will resist the chips and dings associated with production abuse while reducing mark-off and sticking of difficult to process polymers.

High Toughness and Durability: With high toughness, machine downtime due to damaged plugs is reduced. Less downtime = lower costs = more consistent quality.

Good Machinability: No dust collection equipment or respirators are required due to the large, non-abrasive chips.

Excellent Temperature Resistance: HYTAC-B1X is specially formulated for service up to 350°F with minimal loss in mechanical properties.

Variety of Shapes and Sizes: The material is provided in standard sized rods or sheets and may also be custom cut to meet specific needs.

Applications: HYTAC-B1X is a top choice for complex, demanding geometries where clarity and/or material distribution are critical. Excellent where tight plug assist tolerances and plug durability are needed.

Recommended for use with PP, PE, APET, CPET, HIPS, OPS, PETG, PLA, PS, PVC and RPET.

Information Provided by CMT Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.641 - 0.721 g/cc0.0231 - 0.0260 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Flexural Toughness 0.0800 MPa11.6 psi
Compressive Strength 49.0 MPa7100 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 67.7 µm/m-°C37.6 µin/in-°F
Thermal Conductivity 0.180 W/m-K1.25 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 177 °C350 °F
 
Descriptive Properties
ColorLight Blue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CMT Materials HYTAC® XTL Tough Thermoplastic Syntactic Foam
Envalior Pocan® B 1505 000000 PBT
Norplex-Micarta NP500A Epoxy Glass Laminate Sheet, NEMA G-10
CRG Industries Advantic™ 30 Syntactic Foam
Norplex-Micarta MC511A Epoxy Glass Laminate Sheet, NEMA G-11

PCMT007 / 93138

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.