Description: THORNEL® T650 is a continuous, high strength, standard modulus carbon fiber with excellent oxidation resistance and composite performance. THORNEL T650/35 fiber is supplied with 1% UC.309 epoxy compatible sizing.Information provided by Cytec, subsequently acquired by Solvay. |