MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
NRI Titan®-Saturant 100% Solid Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: Titan®-Saturant is a two-part, 100% solid, epoxy system designed for composite laminate repair in conjunction with Titan®, NRI’s infrastructure repair system. It can be used alone, as an anti-corrosion coating, or as a saturant for NRI’s fiberglass system.

Typical Applications:

  • Flare lines, blow down lines, chemical processing lines, firewater lines
  • Girth welds, elbows, tees
  • CUI
  • High temperature environments
Benefits:
  • High temperature rating with an ambient-cured epoxy
  • No heating or post-curing required for typical applications
  • Compatible with a wide range of chemicals as per NRI’s Chemical Compatibility Chart, latest revision.

Information provided by NRI® Innovative Composite Solutions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 670 psiLap, 1,000 hr Hot-Dry Immersion 320°F (160°C)
 837 psiLap, 1,000 hr Hot-Wet Immersion 194°F (90°C)
Adhesive Bond Strength 8.74 MPaLap, to Steel 0.030” (0.76mm) bondline
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 66.0 °C
Minimum Service Temperature, Air 10.0 °C
Glass Transition Temp, Tg 186 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 66.0 °C
Cure to Set
 1.00 min
@Temperature 138 °C
Cure to Set
 3.00 hour
@Temperature 32.0 °C
Cure to Set
 6.00 hour
@Temperature 24.0 °C
Cure to Set
 12.0 hour
@Temperature 16.0 °C
Cure to Set
 24.0 hour
@Temperature 10.0 °C
Cure to Set
 30.0 min
@Temperature 93.0 °C
Cure to Set
Pot Life 75.0 min
Working Life 0.500 min
@Temperature 138 °C
 1.25 hour
@Temperature 24.0 °C
 2.50 hour
@Temperature 16.0 °C
 3.75 hour
@Temperature 10.0 °C
 5.00 min
@Temperature 93.0 °C
 10.0 min
@Temperature 66.0 °C
 35.0 min
@Temperature 32.0 °C
Shelf Life 12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Superior Die Set FORTAL® HP Aluminum Alloy
Superior Die Set FORTAL® HR Aluminum Alloy
Aluminum 7178-T76; 7178-T7651
Aluminum 7001-T75

PNRI031 / 192047

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.