MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Telles M-vera™ B5010 Film Grade Compostable Bioplastic  (discontinued **)
Categories: Polymer; Film; Renewable/Recycled Polymer; Thermoplastic

Material Notes: For use in tough, certified compostable film and bag applications. Mvera B5010 offers a wide range of attractive traits—excellent tear and puncture toughness, excellent seal strength, good printability, translucency—while still processing easily on conventional thermoplastics equipment. Mvera B5010 is designed for the compostable bag and film market where industrial composting is available. Potential uses include blown and cast film applications for industrial can liners, retail bags, organics and yard waste collection bags. Mvera B5010 is certified by Vinçotte to meet EN 13432 composting standards.

Telles is a joint venture between Metabolix and Archer Daniels Midland Company.

Key Words: Mvera
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
Thickness 25.0 microns0.984 milAs tested
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 120 %120 %ASTM D882
Flexural Modulus 0.220 GPa31.9 ksiISO 178
Elmendorf Tear Strength, MD 5.91 g/micron150 g/milASTM D1922
Dart Drop 9.84 g/micron250 g/milASTM D1709
Film Tensile Strength at Break, MD 30.0 MPa4350 psiISO 527
 
Descriptive Properties
ColorWhite

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Telles M-vera™ B5008 Film Grade Compostable Bioplastic
Telles Mirel™ P5001 Film Grade PHA Bioplastic
Telles Mirel™ A5004 Agricultural Film Grade PHA Bioplastic
Telles M-vera™ B5002 Film Grade PHA Bioplastic
Cyclewood Solutions Xylomer™ XM1-KJD Injection Molding Compostable Resin

PMETAA941 / 150414

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.