MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Kraton® D0243 K (SBS) Diblock Copolymer
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Kraton D0243 K is a clear, diblock copolymer based on styrene and butadiene with a polystyrene content of 33%. It is supplied from North America in the physical form identified:
Kraton D0243 KT - supplied as a porous pellet dusted with talc

Region: North America, Asia Pacific, Europe, Japan and South America

Uses: Kraton D0243 K is used as a modifier of bitumen or thermoplastics and in compound formulations. It may also find use as an ingredient in formulating adhesives, sealants and coatings.

Applications: Bitumen Modification; Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and Roofing

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/ccASTM D402
Volatiles <= 1.0 %KM 04
Viscosity 240 - 390 cP25% toluene solution at 25°C; BAM 922
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
Ash 0.35 - 0.75 %Talc; BAM 908
 
Chemical PropertiesOriginal ValueComments
Diblock Content 75 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70
@Time 10.0 sec
Typical values on polymer compression molded at 300°F, Estimated value; ASTM D2240
Tensile Strength 1.72 MPaMeasure of film cast from a solution in toluene, Estimated value; ASTM D412
 
Descriptive Properties
ContentNon-staining phenolic antioxidant0.35-0.48%, KM 08
 Polystyrene31-36%, KM 03
 Total Extractables<1.0%, KM 05
 Vinyl Polybutadiene35%, KM03
Styrene/Rubber Ratio33/67

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® G4610 H (SEBS) with Oil
Kraton® FG1901 + PA-6 blend (20/80)
Kraton® FG1901 + PBT blend (30/70)
Kraton® G1702 + PPE blend (20/80)
Kraton® D1102 B (SBS) Liner Block Copolymer

PKRA9802 / 132701

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.