MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nylene® Nylene 5133 HS Nylon 66, Glass Reinforced, Impact Grade
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Reinforced, Impact Grade

Material Notes: 33% glass fiber reinforced, heat stabilized nylon 6/6. Heat and chemical resistance inherent in nylon resins, while the glass fiber reinforcement gives greatly increased strength and stiffness. Suitable for such applications as brackets, levers, covers, and other uses where strength and stiffness are required. The ASTM line call out is D4066 PA012G33.

Automotive approvals: ASTM D4066 PA0120 G33 ESE-MRD287-B ESE-M4D287-A(non-HS). MS-DB41 CPN3969 (NATURAL) GMP,PA66.013

Testing conducted on dry as molded specimen

Information provided by Nylene® Global Polymer Solutions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccASTM D792
Linear Mold Shrinkage 0.0020 in/in
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 184 MPaASTM D638
Tensile Modulus 9410 MPaASTM D638
Flexural Modulus 8560 MPaASTM D790
Izod Impact, Notched 116 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 262 °CASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 250 °CASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Capron® 5233G 33% Glass-Filled Nylon 66 (Dry)
Celanese Zytel® 70G33L BK031 PA66-GF33
Nylene® Nylene 4114-HS Nylon 66, Impact Grade
Overview of materials for Nylon 66, Unreinforced
Chase Plastics CP Pryme® NN133L (Dry) Nylon 66, 33% Glass Fiber Reinforced, Lubricated

PNYLEN964 / 221496

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.