MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt HUP 12/50 RB-9500 Sheet Molding Compound
Categories: Polymer; Thermoset; Polyester, TS

Material Notes:

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.72 g/cc0.0621 lb/in³ISO 1183 A
Filler Content 50 %50 %ISO 1172
Water Absorption <= 0.30 %<= 0.30 %ISO 62
Linear Mold Shrinkage 0.00050 cm/cm0.00050 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 150 MPa21800 psiISO 527-4
Flexural Strength 300 MPa43500 psiISO 14125
Flexural Modulus 12.0 GPa1740 ksiISO 14125
Tensile Impact Strength 120 kJ/m²57.1 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °C>= 392 °FISO 75
 
Processing PropertiesMetricEnglishComments
Mold Temperature 140 - 155 °C284 - 311 °F
Hold Pressure 8.00 - 12.0 MPa1160 - 1740 psiMolding pressure
Cure Time 1.17 min0.0194 hourISO 12114/1
 
Descriptive Properties
Fiber length25/50 mmPA3.01
Molding time30 s/mm
Surface Weight3000 g/m2ISO 10352

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9161 / 231756

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.