Hostacom ERC 342N E1 C11306 is a 10% talc filled PP copolymer, with excellent impact/stiffness balance, good flowability, very good scratch resistance and outstanding blooming resistance at elevated temperatures. This grade is delivered in C11306 color version. This product is also available in other colors, new colors can be developed depending on customer requirements. Applications: Automotive Parts, Interior TrimsInformation provided by LyondellBasell. |