MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem RP350 Polypropylene Random Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Description: Processing stability, low odor, good flow and set-up behavior, superior clarity, aesthetics and enhanced optical properties, excellent mold release

Applications: Suggested uses include housewares, packaging, containers

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 30.0 MPa50 mm/min; ASTM D638
Elongation at Yield 9.0 %50 mm/min; ASTM D638
Flexural Modulus, 1% Secant 1069 MPa1.3 mm/min; ASTM D790A
Izod Impact, Notched 59.0 J/mASTM D256A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BP Amoco 8410 Polypropylene Random Copolymer
Phillips Sumika Marlex® JM97A Polypropylene Random Copolymer, UV Stabilized
Braskem 6D43 Polypropylene Random Copolymer
Braskem DS6D82 Polypropylene Random Copolymer
Braskem 6D83K Polypropylene Random Copolymer

PBRASK2072 / 199953

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.