Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Low Gloss Uses: Automotive Exterior Parts Automotive Specifications:GM GMP.PVC.013 Form: Pellets Processing Method: Extrusion Information provided by Teknor Apex |