MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Network Polymers Softflex® 0954
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Description: Softflex® Thermoplastic Elastomer Alloy

Information provided by Network Polymers Inc.

A. Schulman has acquired Network Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.032 cm/cm
@Thickness 3.17 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.036 cm/cm
@Thickness 3.17 mm
ASTM D955
Melt Flow 28.9 g/10 min
@Load 1.00 kg,
Temperature 235 °C
Procedure A Condition Q; ASTM D1238
 30.8 g/10 min
@Load 5.00 kg,
Temperature 200 °C
Procedure A Condition G; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 64 - 7410 second dwell; ASTM D2240
 68 - 78Instantaneous; ASTM D2240
Tensile Strength, Yield 1383 psichs 20 in/min; ASTM D412
Elongation at Break 811 %ASTM D412
50% Modulus 0.00257 GPa
@Strain 50 %
ASTM D412
100% Modulus 0.00327 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.00490 GPa
@Strain 300 %
ASTM D412
Gardner Impact >= 320 in-lb
@Temperature -30.0 °C
ASTM D5420
Tear Strength 45.5 kN/mASTM D624
Taber Abrasion, mg/1000 Cycles 0.2382H22 Wheel 1000 g load/1000 cycles; ASTM D3389
Compression Set 78.4 %
@Temperature 70.0 °C
22 hours at 25% deflection; ASTM D395, Method B,
 96.4 %
@Temperature 100 °C
22 hours at 25% deflection; ASTM D395, Method B,
 23.9 %
@Temperature 23.0 °C,
Time 79200 sec
Method B, at 25% deflection; ASTM D395
Tensile Set 7.4 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Diamond ABS/PC 9901
Network Polymers Softflex® 2701
Celanese Celcon® M90™ POM, Unfilled
Celanese Celcon® M90-34 POM, Unfilled
Covestro Makrolon® 2858 Polycarbonate, Injection Grade

PDIAM008 / 29846

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.