Description: Hostacom™ TRC704D medium high melt flow, 1,500 MPa flexural modulus, UV-stabilized thermoplastic elastomeric olefin (TEO) resin has an excellent combination of properties and processability. It was designed for applications that require excellent aesthetics and a good balance of stiffness and impact performance. Information provided by Basell. |