MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Ductile Iron grade 80-55-06
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron; Ductile Iron

Material Notes: Carbon represents the total carbon in the listed composition. Cerium is an optional constituent in ductile iron. Most ductile irons are specified based on mechanical properties and have loosely defined compositions. For example, 80-55-06 ductile iron is specified to have a minimum tensile strength of 80 ksi (552 MPa), a yield strength of 55 ksi (379 MPa) and an elongation of 6%. Ferritic/pearlitic, as cast. Applications include crankshafts, gears and rollers. Hardness and machinability data provided by manufacturer/supplier, Siltin Industries, Inc.

Key Words: UNS F33800, ASTM A536, ferritic, pearlitic, crankshafts, gears, rollers
Vendors: Dura-Bar Metal Services is the leading supplier of Dura-Bar® continuous cast iron and a major distributor of bronze alloys. Our customers rely on us for high quality materials that help increase their profitability. Call us at 1-800-526-0548 or visit dura-barms.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.10 - 7.20 g/cc0.257 - 0.260 lb/in³Typical value of ductile iron
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 187 - 269187 - 269for 80-55-06 T-4 ductile iron.
Hardness, Knoop 254254Converted from Brinell
Hardness, Rockwell C 16.716.7Approximated. Converted from Brinell hardness.
Hardness, Vickers 240240Converted from Brinell
Tensile Strength, Ultimate >= 552 MPa>= 80100 psi
Tensile Strength, Yield >= 379 MPa>= 55000 psi
Elongation at Break 6.0 %6.0 %In 50 mm.
Machinability 0.0 %0.0 %Good machinability. No numerical rating available.
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 3.6 - 3.8 %3.6 - 3.8 %
Cerium, Ce 0.0050 - 0.20 %0.0050 - 0.20 %
Chromium, Cr 0.030 - 0.070 %0.030 - 0.070 %
Copper, Cu 0.15 - 1.0 %0.15 - 1.0 %
Iron, Fe 90.738 - 94.175 %90.738 - 94.175 %
Magnesium, Mg 0.030 - 0.060 %0.030 - 0.060 %
Manganese, Mn 0.15 - 1.0 %0.15 - 1.0 %
Molybdenum, Mo 0.010 - 0.10 %0.010 - 0.10 %
Nickel, Ni 0.050 - 0.20 %0.050 - 0.20 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si 1.8 - 2.8 %1.8 - 2.8 %
Sulfur, S <= 0.0020 %<= 0.0020 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ductile Iron grade 65-45-12
Ductile Iron grade 60-40-18
Ductile Iron grade 100-70-03
Ductile Iron grade 80-60-03
Gray Cast Iron, ASTM A 48 Class 40

MDFE05 / 12002

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.