MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Phillips 66 COPYLENE® CH034EV Polypropylene, Homopolymer, Fiber, Tape, UV  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Fiber Grade

Material Notes: COPYLENE™ CH034EV is a polypropylene homopolymer resin designed for fiber applications. Applications: Filament Yarn, Geotextile & agriculture. Equivalent to Pro-fax® HL348J

Information provided by Phillips 66.

Key Words: Filament Yarn, Geotextile & agriculture
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.902 g/ccASTM D792
Melt Flow 3.4 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 5300 psi2 in/min; ASTM D638
Elongation at Yield 11 %ASTM D638
Flexural Modulus, 1% Secant 210000 psi0.05 in/min; Procedure A; ASTM D790
Izod Impact, Notched 0.800 ft-lb/in
@Temperature 23.0 °C
Method A; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °Cunannealed; ASTM D648
 
Descriptive Properties
ProcessFiber

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Polystrand ThermoPro™ IE6010 Unitape Unidirectional Polypropylene-Glass Composite
Ineos H05H-01 Polypropylene Homopolymer
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
Phillips 66 COPYLENE® CH008 Polypropylene, Homopolymer, Netting
Bamberger Polymers Bapolene® 4062 Polypropylene, Injection Grade

PCOPY013 / 100809

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.