MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LATI Latamid 66 B G/20-V PA 66, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Glass Fiber Filled; Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: Polyamide 66 (PA66) based compound. High fluidity. Glass fibers. Flame retardant, non classifiable, with brominated flame retardants, PBB/PBDE free.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.52 g/cc
Linear Mold Shrinkage, Flow 0.0025 - 0.0045 cm/cm
Linear Mold Shrinkage, Transverse 0.0070 - 0.010 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.0 MPa
@Temperature 150 °C
 50.0 MPa
@Temperature 120 °C
 60.0 MPa
@Temperature 90.0 °C
 75.0 MPa
@Temperature 60.0 °C
 115 MPa
@Temperature 23.0 °C
Elongation at Break 2.5 %
@Temperature 23.0 °C
 4.0 %
@Temperature 60.0 °C
 5.0 %
@Temperature 90.0 °C
 5.3 %
@Temperature 120 °C
 6.0 %
@Temperature 150 °C
Elongation at Yield 3.0 %
@Temperature 60.0 °C
 4.5 %
@Temperature 90.0 °C
 4.8 %
@Temperature 120 °C
 5.5 %
@Temperature 150 °C
Tensile Modulus 2400 MPa
@Temperature 150 °C
 3200 MPa
@Temperature 120 °C
 4000 MPa
@Temperature 90.0 °C
 5800 MPa
@Temperature 60.0 °C
 8100 MPa
@Temperature 23.0 °C
Charpy Impact Unnotched 25.0 kJ/m²
@Temperature -20.0 °C
 30.0 kJ/m²
@Temperature 23.0 °C
Charpy Impact, Notched 2.80 kJ/m²
@Temperature -20.0 °C
 3.50 kJ/m²
@Temperature 23.0 °C
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 250 VA solution
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 90.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 235 °C
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
Vicat Softening Point 220 °C
@Load 5.00 kg
Flammability, UL94 V-0
@Thickness 3.00 mm
 V-0
@Thickness 1.50 mm
 V-0
@Thickness 0.750 mm
Oxygen Index 33 %
Glow Wire Test 960 °C
@Thickness 1.00 mm
GWFI/GWT
 960 °C
@Thickness 2.00 mm
GWFI/GWT
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 - 280 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 90.0 - 100 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LATI Latamid 66 PA 66
BASF Ultramid® A3WG7 35% Glass Filled PA66 (Dry)
Celanese Zytel® BM70G20HSLX BK537 PA66-IGF20
LATI Latamid 66 E21 G/30 PA 66, 30% Glass Fiber Reinforced
LATI Latiohm 66-05 PD01 G/20 PA66, 20% Glass Fiber Reinforced

PLATH9700 / 177396

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.