MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ohio Carbon Blank OCB UT-3 Mechanical Grade Graphite
Categories: Carbon; Graphite

Material Notes: Available in a range of sizes and shapes.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Apparent Bulk Density 1.70 g/cc0.0614 lb/in³
Particle Size 10.2 µm10.2 µmAverage
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5050
Tensile Strength 20.7 MPa3000 psi
Flexural Strength 36.5 MPa5300 psi
Compressive Strength 68.9 MPa10000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00135 ohm-cm0.00135 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 93.4 W/m-K648 BTU-in/hr-ft²-°F
 
Descriptive Properties
GrainFine
Suggested ApplicationsForging Dies
 Large Cavity Molds
 Large Die Casts
 Large Extrusion Dies
 Roughing Electrodes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Graphite, Carbon, C
Aremco Graphi-Bond™ 551-R
Aremco Graphi-Bond™ 551-RN High Temperature Ceramic Adhesive/Paste, Graphite Filled
Aremco Graphi-Bond™ 669 High Temperature Ceramic Adhesive/Paste, Graphite Filled
Aremco Pyro-Paint™ 634-CA High Temperature Refractory Coating

EOHIOCA88 / 108533

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.