MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Evonik Vestamid® DX9320 Black 10% Glass Reinforced Nylon 612 (Dry as Molded)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Glass Fiber Filler

Material Notes: Description: impact-resistant, 10% glass fiber reinforced, medium-viscosity, heat-stabilized

Applications: housings subject to impact, coverings with molded-on elastomer seals

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Key Words: PA612-HI, MH, 14-040, GF10
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.0 %1.0 %23°C/50% R.H.; ISO 62
Water Absorption at Saturation 2.6 %2.6 %ISO 62
Linear Mold Shrinkage 0.0129 cm/cm0.0129 in/in127x12.7x3.2 mm (processing cond. acc. To DIN EN ISO 1874-2)
Linear Mold Shrinkage, Transverse 0.0097 cm/cm0.0097 in/in127x12.7x3.2 mm (processing cond. acc. To DIN EN ISO 1874-2)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 82.0 MPa11900 psiISO 527-2/1A
Elongation at Break 10 %10 %ISO 527-2/1A
Tensile Modulus 3.70 GPa537 ksiISO 527-2/1A
Charpy Impact Unnotched  6.90 J/cm²
@Temperature -30.0 °C
32.8 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 8.10 J/cm²
@Temperature 23.0 °C
38.5 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.10 J/cm²
@Temperature 23.0 °C
5.24 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Dielectric Constant  3.1
@Frequency 1e+6 Hz
3.1
@Frequency 1e+6 Hz
IEC 60250
 4.3
@Frequency 100 Hz
4.3
@Frequency 100 Hz
IEC 60250
Dissipation Factor  0.0466
@Frequency 1e+6 Hz
0.0466
@Frequency 1e+6 Hz
IEC 60250
 0.047
@Frequency 100 Hz
0.047
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index >= 600 V>= 600 VTest Solution A, 50 drops; IEC 60112
 600 V600 VTest Solution A, 100 drops; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 131 °F
Longitudinal; ISO 11359
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359
Melting Point 215 °C419 °FPeak Temperature; ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 201 °C394 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 183 °C361 °FISO 75
Vicat Softening Point 199 °C390 °F50N; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, Impact Modified
Sandvik Osprey S2 Tool Steel Powder (Grade 95% - 16)
PSM Industries PolyAlloys MIM-430L sintered Stainless Steel
Kinetics MIM 4605 Low Alloy Steel (Austempered)

PHULA11 / 47371

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.