MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Huntsman IROGRAN® A 85 P 4722 TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: IROGRAN A 85 P 4722 is a halogen-free thermoplastic- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are good microbial resistance, high low-temperature flexibility, especially suitable for the substructure in cable construction.

Performance Features:

  • Good hydrolysis resistance
  • Excellent processability
  • Good abrasion resistance
  • Halogen free
Applications: For the production in jacket construction.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccInjection molded parts
Melt Index of Compound 100 g/10 min
@Load 21.6 kg,
Temperature 190 °C
MVR, [cm3/10 min]
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85Injection molded parts; ASTM D2240
Tensile Strength at Break >= 35.0 MPaInjection molded parts; DIN 53504
Elongation at Break >= 600 %Injection molded parts; DIN 53504
Abrasion <= 30mm3, Injection molded; ISO 4649
 
Processing PropertiesOriginal ValueComments
Feed Temperature 25.0 - 40.0 °CExtrusion
Middle Barrel Temperature 165 - 190 °CExtrusion
Nozzle Temperature 170 - 200 °CExtrusion
 180 - 200 °CInjection
Adapter Temperature 175 - 195 °CExtrusion
Die Temperature 175 - 200 °CExtrusion
Melt Temperature 170 - 195 °CInjection
Mold Temperature 20.0 - 70.0 °CInjection
 
Descriptive Properties
Heating Zone175-195°CInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLTHANE® 11T93 Thermoplastic Polyurethane Elastomer
Lubrizol Estane® S190A Thermoplastic Polyurethane
Lubrizol Advanced Materials PEARLTHANE® 16N80 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 11T85UV Thermoplastic Polyurethane Elastomer
Huntsman IROGRAN® A 95 K 4977 TPU-High Temperature Performance

PHUQ102 / 159475

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.