MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC FLEX NORYL™ Resin WCD883CU Polyphenylene Ether + TPE (PPE+TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyphenylene Ether/PPO

Material Notes: FLEX NORYL™ WCD883CU resin is a flexible, non-reinforced extrudable blend of Polyphenylene Ether (PPE) + Thermoplastic Elastomer (TPE). This UV stabilized material contains non-halogenated flame retardant and performance capable of meeting EN 50265-2-1 requirements. FLEX NORYL WCD883CU resin was developed for evaluation in AC cable jacket applications such as HD 21.14 flexible cables that require EU VDE and light color. It has a Shore A Hardness reading of 88 and exhibits superior thermal stability, very low water absorption, good electric properties, and low specific gravity. Processing is typically conducted on standard extrusion equipment, and UL 1581 testing is conducted on 2.0mm wire with 0.12mm X 20 stranded copper conductor.

Features: Flexible,Hydrolytic Stability,Low Creep Sensitivity,Flame Retardant,Thin Wall,Non-Halogenated,Non-Chlorinated,Non-Brominated,Good Processability,Ductile

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Moisture Absorption 0.0200 %Wire Coating Extrusion
Melt Flow 10 g/10 min
@Load 10.0 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 8830s reading; ASTM D2240
Tensile Strength at Break 12.5 MPa50 mm/min; ISO 527
 14.0 MPa50 mm/min; ASTM D638
 18.0 MPaUL 1581
 19.0 MPaafter 7days @80°C; UL 1581
Elongation at Break 135 %50 mm/min; ISO 527
 160 %50 mm/min; ASTM D638
 238 %after 7days @80°C; UL 1581
 260 %UL 1581
Flexural Modulus 61.0 MPa12.5 mm/min; ISO 178
 65.0 MPa12.5 mm/min, 100 mm span; ASTM D790
Heat Distortion 22 %
@Load 0.250 kg,
Temperature 100 °C
UL 1581
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.20e+15 ohm-cmASTM D257
Surface Resistance 1.70e+16 ohmASTM D257
Dielectric Constant 3.0
@Frequency 1.10e+9 Hz
SABIC method
Dielectric Strength 25.0 kV/mm
@Thickness 2.00 mm
in oil; IEC 60243-1
Dissipation Factor 0.0030
@Frequency 1.10e+9 Hz
SABIC method
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -40.0 °CASTM D746
Oxygen Index 36 %ISO 4589
Glow Wire Ignition Temperature 775 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 15.0 - 60.0 °CWater Bath Temperature
 220 - 250 °CNeck Temperature
Feed Temperature 180 - 220 °C
Middle Barrel Temperature 220 - 250 °C
Die Temperature 220 - 250 °CWire Coating Extrusion
Melt Temperature 220 - 250 °CWire Coating Extrusion
Head Temperature 220 - 250 °CCross-head Temperature
 220 - 250 °C
Wire Preheat Temperature 25.0 - 120 °C
Drying Temperature 75.0 - 85.0 °CWire Coating Extrusion
Dry Time 5.00 - 7.00 hourWire Coating Extrusion
 12.0 hourCumulative; Wire Coating Extrusion
Screw Speed 15 - 85 rpm
 
Descriptive Properties
Cooling Water Air Gap100-200 mm
Extruder Length/Diameter Ratio (L/D)22:1 to 26:1
Screen Pack100-150
Vertical Flame TestPassesEN 50265-2-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82081 / 290028

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.