MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Aperam Supera 40 Cold Rolled Strip
Categories: Metal; Ferrous Metal

Material Notes: SUPRA 40 is an iron-nickel soft magnetic alloys with maximum saturation induction and high permeability with very good stampability. Main applications are clock motors parts, CTR gun grids.

International standards: JIS C 2531

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.15 g/cc0.294 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 130130Annealed
 225225Hard Temper
Tensile Strength 500 MPa72500 psiAnnealed
 700 MPa102000 psiHard Temper
Elongation at Break 3.0 %3.0 %Hard Temper
 30 %30 %Annealed
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.0000063 ohm-cm0.0000063 ohm-cm
Magnetic Permeability <= 66000
@Thickness 0.350 mm
<= 66000
@Thickness 0.0138 in
DC
Magnetic Coercive Force, Hc 0.075 Oe
@Thickness 0.350 mm
0.075 Oe
@Thickness 0.0138 in
Magnetic Saturation Flux Density, Bmax 14500 Gauss
@Thickness 0.350 mm
14500 Gauss
@Thickness 0.0138 in
DC, Saturation Induction
Curie Temperature 330 °C626 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.50 µm/m-°C2.50 µin/in-°F
Specific Heat Capacity 0.500 J/g-°C0.120 BTU/lb-°F
Thermal Conductivity 12.5 W/m-K86.8 BTU-in/hr-ft²-°F
Melting Point 1425 °C2597 °F
 
Component Elements PropertiesMetricEnglishComments
Iron, Fe 59 %59 %
Nickel, Ni 41 %41 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aperam AFK 502R Cold Rolled Strip
Aperam Supermimphy® L Cold Rolled Strip
FloMet Fe-3% Si Soft Magnetic Alloy
Aperam Permimphy SP Cold Rolled Strip
Ferrite 1, Sintered Iron-Barium Oxide Hard Magnetic Material

NPERA013 / 194802

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.