MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), 40% Glass Fiber

Material Notes: Polyetherimide, 40% Glass Reinforced

Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Key Words: UL E113219
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.60 g/ccASTM D792
Water Absorption 0.13 %
@Time 86400 sec
ASTM D570
Moisture Absorption at Equilibrium 0.90 %ASTM D570
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cmASTM D955
Melt Flow 3.0 - 18 g/10 min
@Load 6.70 kg,
Temperature 337 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 114ASTM D785
Tensile Strength at Break 25600 psiASTM D638
Tensile Strength, Yield 25600 psiASTM D638
Elongation at Break 2.5 %ASTM D638
Tensile Modulus 1.69e+6 psiASTM D638
Flexural Strength 34000 psiASTM D790
Flexural Modulus 1600 ksiASTM D790
Izod Impact, Notched 1.80 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Izod Impact, Unnotched 8.00 ft-lb/in
@Temperature 22.8 °C
ASTM D4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.50e+16 ohm-cmASTM D257
Dielectric Constant 3.7
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 600 V/milin oil; ASTM D149
Dissipation Factor 0.0020
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.00 µin/in-°F
@Temperature -20.0 - 150 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 418 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 413 °FASTM D648
Vicat Softening Point 450 °F120°C/h, 50 N; ASTM D1525
UL RTI, Electrical 221 °F
@Thickness 1.50 mm
UL 746
 221 °F
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 221 °F
@Thickness 1.50 mm
UL 746
 221 °F
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 221 °F
@Thickness 1.50 mm
UL 746
 221 °F
@Thickness 3.00 mm
UL 746
Flammability, UL94 V-0
@Thickness 1.50 mm
 V-0
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 630 - 750 °F
Middle Barrel Temperature 640 - 750 °F
Front Barrel Temperature 650 - 750 °F
Melt Temperature 640 - 750 °F
Mold Temperature 225 - 350 °F
Drying Temperature 290 - 300 °F
Dry Time 3.00 - 4.00 hour
Vent Depth 0.00100 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLYQ198 / 160719

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.