MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC VALOX™ FR DR48 PBT (Americas)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: VALOX DR48 is a 17% glass filled, flame retardant Polybutyleneterephthalate (PBT) injection moldable grade with excellent chemical resistance. It has a UL94V0@0.90mm and 5VA@3.0mm flame rating. This is a good candidate for a variety of applications in the electrical industry including connectors, bobbins, and switches.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.53 g/ccASTM D792
 1.53 g/ccASTM D792
Water Absorption 0.070 %24 hours; ASTM D570
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
@Thickness 1.50 - 3.20 mm
SABIC method
 0.0060 - 0.0090 cm/cm
@Thickness 3.20 - 4.60 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0080 cm/cm
@Thickness 1.50 - 3.20 mm
SABIC method
 0.0080 - 0.011 cm/cm
@Thickness 3.20 - 4.60 mm
SABIC method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118ASTM D785
Tensile Strength at Break 93.0 MPa5 mm/min; ASTM D638
Flexural Strength 140 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 5200 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 49.0 J/mASTM D256
Izod Impact, Unnotched 500 J/mASTM D4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.4
@Frequency 1e+6 Hz
ASTM D150
 3.6
@Frequency 100 Hz
ASTM D150
Dielectric Strength 18.8 kV/mm
@Thickness 3.20 mm
in air; ASTM D149
 25.0 kV/mm
@Thickness 1.60 mm
in oil; ASTM D149
Dissipation Factor 0.0020
@Frequency 100 Hz
ASTM D150
 0.016
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 175 - 250 VUL 746A
Hot Wire Ignition, HWI 15 - 30 secUL 746A
High Amp Arc Ignition, HAI >= 120 arcsUL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 19.8 µm/m-°C
@Temperature 60.0 - 138 °C
ASTM E831
 19.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Hot Ball Pressure Test 125 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 182 °C
@Thickness 6.40 mm
unannealed; ASTM D648
UL RTI, Electrical 120 °CUL 746B
UL RTI, Mechanical with Impact 120 °CUL 746B
UL RTI, Mechanical without Impact 140 °CUL 746B
Flammability, UL94 V-0
@Thickness 0.900 mm
UL 94
 5VA
@Thickness 3.00 mm
UL 94
Oxygen Index 29 %ASTM D2863
Glow Wire Test 700 °C
@Thickness 1.00 mm
IEC 60695-2-13
 725 °C
@Thickness 3.00 mm
IEC 60695-2-13
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 245 - 260 °CInjection Molding
Zone 1 240 - 255 °C
Zone 2 245 - 260 °C
Zone 3 250 - 265 °C
Melt Temperature 250 - 265 °C
Mold Temperature 65.0 - 90.0 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 12.0 hourCumulative; Injection Molding
Moisture Content 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 80 %
Vent Depth 0.00250 - 0.00380 cm
Screw Speed 50 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10345 / 243812

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.