MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
NeXolve Novastrat® 800 Polyimide
Categories: Polymer; Film; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: High temperature polyimide film with low coefficient of thermal expansion.

NeXolve Novastrat® 800 is a high temperature polyimide film with low coefficient of thermal expansion (CTE), ~4 ppm/°C from -140 °C to +225 °C, that closely matches the CTE of many metals and metal oxides. Novastrat® 800 has been successfully used in applications requiring the stability of low CTE from cryogenic conditions (less than -150 °C, -238 °F) to very high temperatures (greater than 250 °C, 482 °F).

Novastrat® 800 is a recommended grade for applications that require low CTE and stable properties across a wide range of operating temperatures. Novastrat® 800 is provided as a film in sheet form, or liquid resin for spray or flow casting operations. As a liquid, it bonds well to metals and metal oxides, and is supplied with and without a variety of internal adhesion promoters.

Information Provided by NeXolve Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 272 MPa
@Thickness 0.0178 mm
ASTM D882-02
Elongation at Break 6.0 %
@Thickness 0.0178 mm
ASTM D882-02
Tensile Modulus 8.00 GPa
@Thickness 0.0178 mm
ASTM D882-02
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.00 µm/m-°C
@Thickness 1.00 mm,
Temperature -125 - 20.0 °C
ASTM E831-06
Glass Transition Temp, Tg 341 °CDSC; ASTM E1356-03
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.62
@Wavelength 549 nm
Abbe; ASTM D542-00
UV Transmittance 50 %
@Thickness 0.0178 mm,
Wavelength 438 nm
50% Transmission UV Cutoff
 
Descriptive Properties
ApplicationsAdvanced Composites
 Electrical Insulators
 Industrial Tapes
 Space Structures
 Thermal Insulation
CharacteristicsBonds directly to metals and metal oxides
 Conductive and non-conductive grades
 High heat stability
 Low coefficient of thermal expansion
Solar Absorptivity0.10.7 mil thickness; ASTM E903-96

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Vespel® SF-0920 Polyimide Foam, Low Density
NeXolve Clear Optionox® Polyimide Film/Coating
NeXolve Novastrat® 905 Polyimide
NeXolve Thermalbright® C Polyimide Film
NeXolve Thermalbright® N Polyimide Film

PNEXOL912 / 171866

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.