MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Oceanchem Group Melamine Polyphosphate (MPP)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Cas No.: 20208-95-1

Use: Mainly used in polyamide and PBT, especially PA6, PA66, glass fiber-reinforced PA6, PA66. Nylon containing FR-NP can be used in all kinds of injection and extrusion processes and meets all processing demands of polyamide, glass fiber polyamide.

    Features
  • Halogen-free and low poison, meet European Environmental Protection requirements
  • Easy process, no need special screws combination and special specification glass fiber
  • Different from general halogen retardant, no corrosion damage to equipment and mold
  • Good het stability, decomposition temperature=330°C, suitable for glass fiber-reinforced nylon
  • Flame retardant products containing FR-NP can be made to various color
Storage and Transportation: Handle with care, keep air-tight and dry.

Information Provided by Oceanchem Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 1.50 g/cc
Density 1.60 g/cc
Particle Size 25 µm
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature 330 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content 0.20 %
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 15.01 %
 
Descriptive Properties
AppearanceFine, white, crystalline powder
CAS Number20208-95-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chengdu Polyster RPM540B Flame Retardant Masterbatch
Arkema LOTADER® AX 8900 Terpolymer Ethylene - Acrylic Ester - Glycidyl Methacrylate
Lanxess STABAXOL® KE 9193 Masterbatch Antihydrolysis agent
Lanxess Uniplex FRP-64 Plastic Additive
M Chemical GUARD DOG™ UV1577 Light Absorber, Triazene Derivative

POCEAN20 / 104224

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.