MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond Supreme 12AOHT-LO One Component Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, High Temperature

Material Notes: Key Features:
  • Cryogenically serviceable
  • Superior ability to withstand thermal cycling
  • Convenient handling, no mixing and no freezing
  • Excellent bonding and physical strength properties
  • High temperature resistant
  • Exceptionally low shrinkage upon curing
Product Description: Master Bond Supreme 12AOHT-LO has an impressive combination of easy and straightforward processing along with an array of superb properties after curing. It is a single component system that cures at 125°C (257°F) in 60-70 minutes and 150°C (302°F) in 40-50 minutes. There is no need for it to be stored frozen. Additionally, it has unlimited working life at room temperature. Upon cross-linking, Supreme 12AOHT-LO has numerous favorable attributes highlighted by excellent thermal conductivity, superior electrical insulation and the ability to withstand rigorous thermal cycling. It bonds well to a wide variety of substrates, including metals, composites, glass, ceramics and many plastics. This epoxy has formidable bond strength, particularly in the shear mode, exceeding 3,500 psi. The service temperature range is eye-catching, extending from 4K to +500°F. Also, it truly qualifies as a NASA low outgassing system. Along with the attractive profile, this structure has superlative dimensional stability and a robust aggregation of physical strength properties. Supreme 12AOHT-LO is a toughened system with superior resistance to aggressive thermal cycling and shock. It is notable for its dimensional stability and its impressive array of physical strength properties. Supreme 12AOHT-LO has ample chemical resistance, particularly to water, oil, fuels and solvents. It is gray in color. Supreme 12AOHTLO is a compelling choice for bonding and sealing in aerospace, electronic, electro-optic, specialty OEM as well as for vacuum environments, where the combination of convenient processing and handling along with the extensive performance profile discussed previously is highly desirable.

Product Advantages:

  • Single component system; no mixing prior to use
  • Unlimited working life at room temperature
  • High bond strength, particularly lap shear
  • Extraordinary temperature range from 4K to +500°F
  • Fully meets ASTM E595 for low outgassing
  • Capable of withstanding rigorous thermal cycling
  • Combines excellent electrical insulating values along with substantial thermal conductivity

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Storage Temperature 7.22 - 12.8 °C45.0 - 55.0 °Ffor max shelf life
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 85>= 85
Tensile Strength >= 55.2 MPa>= 8000 psi
Tensile Modulus 3.79 - 4.14 GPa550 - 600 ksi
Compressive Strength >= 152 MPa>= 22000 psi
Adhesive Bond Strength >= 24.1 MPa>= 3500 psiTensile Lap, Aluminum to Aluminum
Peel Strength 0.877 - 1.75 kN/m5.00 - 10.0 plialuminum to aluminum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 4.4
@Frequency 60 Hz
4.4
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.30 - 1.44 W/m-K9.00 - 10.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -167 °C-269 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  40.0 - 50.0 min
@Temperature 149 °C
0.667 - 0.833 hour
@Temperature 300 °F
 60.0 - 70.0 min
@Temperature 121 °C
1.00 - 1.17 hour
@Temperature 250 °F
Shelf Life 3.00 - 6.00 Month3.00 - 6.00 Monthin original, unopened containers
 
Descriptive Properties
ViscositySmooth, thixotropic paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP113 Two Component Epoxy
Master Bond EP121AO Thermally Conductive, Dimensionally Stable Epoxy System
Master Bond EP46HT-2ND2 Two Part Epoxy
Master Bond EP46HT-1ND2 Two Component Epoxy
Master Bond EP42HT-2FG Two Component Epoxy Adhesive for Food Applications

PMASTM960 / 185553

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.