MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical SEETEC H5300 Polypropylene, Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Features: Seetec H5300 is designed for the extrusion of textile yarn and monofilaments. This grade is characterized by good processability and stretchability. SEETEC H5300 meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520 for food contact.

Applications: Woven fabric, carpet backing, rope, split yarn

CAS No. 9003-07-0

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/ccASTM D1505
Melt Flow 3.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100ASTM D785
Tensile Strength, Yield 350 kg(f)/cm²50mm/min; ASTM D638
Elongation at Break <= 500 %50mm/min; ASTM D638
Flexural Modulus 15000 kg(f)/cm²ASTM D760
Izod Impact, Notched 3.00 kg-cm/cm
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 140 - 170 °C
Deflection Temperature at 0.46 MPa (66 psi) 104 °CASTM D648
Vicat Softening Point 152 °C
@Load 1.00 kg
ASTM D1525
Flash Point >= 340 °C
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical SEETEC H1500 Polypropylene Homopolymer
LG Chemical SEETEC H1501 Polypropylene Homopolymer
LG Chemical SEETEC H7411 Polypropylene, Homopolymer
LG Chemical SEETEC M1600 Polypropylene Impact Copolymer
LG Chemical SEETEC H7511 Polypropylene, Homopolymer

PLAY378 / 148388

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.