Hostalen PP H2222 36 is a polypropylene block copolymer grey colored similar to RAL 7032 (pebble grey) and is typically used in the applications of filter plates. Applications: Industrial, Plumbing, Heating & CoolingInformation provided by LyondellBasell. |