MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Epsan Eplamid 6 GFI 15 NC Q1B5A801 Polyamide 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: Reinforced with 15% of glass fiber and modified polyamide 6, with improved impact resistance, heat stabilized for injection molding. Used in all sectors of industry, offering a good impact strength for mechanical properties and ensuring outstanding performance even at low temperatures (up to -23°C).

Information provided by Epsan Plastik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Linear Mold Shrinkage 0.0050 cm/cmParallel; ISO 294-4
 0.0090 cm/cmNormal; ISO 294-4
Ash 15 %ISO 3451-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 60.0 MPaConditioned; ISO 527-2
 100 MPaDry; ISO 527-2
Elongation at Break 5.0 %Dry; ISO 527-2
 15 %Conditioned; ISO 527-2
Tensile Modulus 3100 MPaConditioned; ISO 527-2
 5000 MPaDry; ISO 527-2
Flexural Strength 90.0 MPaConditioned; ISO 178
 155 MPaDry; ISO 178
Flexural Modulus 2600 MPaConditioned; ISO 178
 4400 MPaDry; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²ISO 180/1A
Charpy Impact, Notched 17.0 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 210 °CISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 190 °CISO 75-2/A
Vicat Softening Point 205 °CISO 306/B50
Flammability, UL94 HB
@Thickness 1.60 mm
EN 60695-11-10
 
Processing PropertiesOriginal ValueComments
Processing Temperature 260 °CRecommended Injection Molding Temperature
Drying Temperature 80.0 °CAverage Drying Time is 2-4 hrs
Moisture Content 0.20 %ISO 15512

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epsan Eplamid 66 GFI 15 NC Q1B5A601 Polyamide 66
Clariant 6618G15 HSL UV Black Nylon 66, 15% Glass Fiber, Impact Modified, UV and Heat Stabilized, Lubricated
A. Schulman SCHULAMID® 6 GF15H 15% Glass Fiber Reinforced, Heat Impact Nylon 6
Clariant Renol PA123G13 Nylon 66, 13% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated
Envalior Durethan® BKV 115 H3.0 000000 Nylon 6-Copolymer, Glass Fiber Reinforced

PEPSAN020 / 186334

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.