MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Rhyolite-Andesite
Categories: Ceramic

Material Notes: Rhyolite is an igneous rock with a fine texture and grain size < 1 mm (extrusive). It is acidic, with a total silica content greater than 65%. Andesite is generally darker in color than felsite.

Property values are typical of Rhyolite-Andesite used in construction. Actual property values will vary from sample to sample.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.20 - 2.50 g/cc0.0795 - 0.0903 lb/in³
Porosity 4.0 - 15 %4.0 - 15 %
Permeability 1.0e-8 - 0.0101.0e-8 - 0.010Aggregation property, d (µ = (-log d))
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 5.0 - 6.55.0 - 6.5
Modulus of Rupture 0.00100 - 0.0700 GPa0.145 - 10.2 ksi
Compressive Strength 60.0 - 220 MPa8700 - 31900 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.00 - 9.00 µm/m-°C
@Temperature 20.0 °C
2.78 - 5.00 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.800 - 3.80 W/m-K5.55 - 26.4 BTU-in/hr-ft²-°F

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Granite
Andesite
Basalt
Breccia, Volcanic
Diorite

BMIN116 / 226

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.