Notes: Monprene CP-37942 is a general purpose thermoplastic elastomer designed for a variety of consumer product applications requiring a soft, rubber-like feel. Monprene CP-37942 is a high density, medium hardness grade that exhibits excellent anti-vibration characteristics. This grade is suitable for injection molding and extrusion. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Filled; High Density; High Specific Gravity; Light Stabilized; Low Flow; Medium Hardness; UV Resistant; Weather Resistant Uses: Agriculture Applications; Appliance Components; Consumer Applications; Flexible Grips; Gaskets; Grommets; Handles; Knobs; Plugs; Profiles; Rubber Replacement; Sporting Goods; White Goods & Small Appliances RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding; Extrusion Information provided by Teknor Apex |