MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives CoolTherm™ EP-343 Thermally Conductive Epoxy Conformal Coating
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: LORD CoolTherm™ EP-343 coating is a two-component, dielectric epoxy coating recommended for coating printed circuit boards, semiconductors and heat sink assemblies. CoolTherm EP-343 coating efficiently distributes heat from the circuits throughout the coated surface of the board.

Features: provides high electrical insulation with exceptionally good heat transfer. provides good resistance to water and a wide variety of chemicals. can be used on parts and devices that experience operating temperatures from -65°C to +130°C. maintains low viscosity, allowing easy application with conventional spray equipment. meets requirements of Military Specification MIL-E-5272. cured system is free of dimpling; provides good edge coverage and excellent hiding power, even in thin applications.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.990 g/ccEP-343 Hardener
 1.35 g/ccMixed
 1.41 g/ccEP-343 Resin
Water Absorption 0.20 %
@Temperature 25.0 °C,
Time 864000 sec
cured
Viscosity 55 cP
@Temperature 25.0 °C
EP-343 Hardener
 55 cP
@Temperature 25.0 °C
Mixed
 65 cP
@Temperature 25.0 °C
EP-343 Resin
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90cured
Tensile Strength 8300 psi
@Temperature 25.0 °C
cured
Elongation at Break 1.9 %cured
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cm
@Temperature 25.0 °C
cured; ASTM D 257
Dielectric Constant 5.6
@Frequency 100000 Hz,
Temperature 25.0 °C
cured
Dielectric Strength 1500 V/mil
@Thickness 0.0762 mm
cured
Dissipation Factor 0.020
@Frequency 100000 Hz,
Temperature 25.0 °C
cured
 
Thermal PropertiesOriginal ValueComments
CTE, linear 24.0 µm/m-°Ccured; ASTM C 864
Thermal Conductivity 1.10 W/m-Kcured
Maximum Service Temperature, Air 130 °C
Minimum Service Temperature, Air -65.0 °C
Glass Transition Temp, Tg 106 °Ccured
 
Processing PropertiesOriginal ValueComments
Working Life 1440 min
@Temperature 25.0 °C
Mixed
Shelf Life 12.0 Month
@Temperature 25.0 °C
EP-343 Resin
 24.0 Month
@Temperature 25.0 °C
EP-343 Hardener
 
Descriptive Properties
AppearanceAmber LiquidEP-343 Hardener
 Black LiquidEP-343 Resin
 Black LiquidMixed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Resinlab® EP1320 Heat Cure Epoxy Conformal Coating
Master Bond EP41S-1 Chemically Resistant Two Component Epoxy System
Lord Adhesives CoolTherm™ EP-6968 Conductive Adhesive System
Wacker Semicosil® 964 Conformal Coating
Tra-Con Tra-Bond 2151T Thermally Conductive Electrically Insulating Compound

PLORD9286 / 232642

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.